Hydrofluoric acid concentration and etching time on bond strength to lithium disilicate glass-ceramic . Research, Society and Development, [S. l.], v. 10, n. 17, p. e215101724776, 2021. DOI: 10.33448/rsd-v10i17.24776. Disponível em: https://ojs34.rsdjournal.org/index.php/rsd/article/view/24776. Acesso em: 28 jun. 2025.